The OID 98122319-57000mAh-3.65V-3C-0112 is a premium single-cell lithium-ion polymer battery engineered by Shenzhen Jianheng Technology Co Ltd for applications that demand extreme capacity, long endurance and high discharge rate capability. With a typical capacity of 57.0Ah and a minimum capacity of 55.0Ah, this cell delivers reliable power for electric vehicles, energy storage systems and high-performance UAV platforms.
\nBuilt with an aluminum plastic film shell and advanced electrode technology, the OID 98122319 achieves an ultra-low AC impedance of no more than 1.0mΩ at 1kHz (58% SOC), enabling high continuous discharge currents up to 3.0C and pulse currents up to 8.0C for 10 seconds. This makes it an ideal choice for drone battery packs, eVTOL systems and other high-power applications requiring stable performance and long cycle life.
\n\n| Parameter | Value | Note |
|---|---|---|
| Capacity (Typical) | 57.0Ah | 0.5C at 4.2V to 2.75V at 25±2°C |
| Capacity (Minimum) | 55.0Ah | 0.5C at 4.2V to 2.75V at 25±2°C |
| Nominal Voltage | 3.65V | 0.5C at 4.2V to 2.75V at 25±2°C |
| AC Impedance (ACIR) | ≤1.0mΩ | At 1kHz, 58% SOC, 25±2°C |
| Charge Cut-off Voltage | 4.2V | |
| Discharge Cut-off Voltage | 2.75V | |
| Standard Charge Method | 0.5C CC to 4.2V, 4.2V CV to 0.05C | |
| Standard Discharge Method | 0.5C | |
| Maximum Charge Current | 2.0C | Continuous |
| Maximum Discharge Current | 3.0C | Continuous |
| Maximum Pulse Discharging Current | 5.0C/10s at SOC >60%; 8.0C/10s at SOC >70% | |
| Operating Temperature - Charge | 0~5°C: 0.1C max; 6~15°C: 0.2C max; 16~24°C: 0.5C max; 25~35°C: 2.0C max; 36~45°C: 0.5C max | Charge to 4.2V |
| Operating Temperature - Discharge | -20°C to 55°C | |
| Storage Temperature | 12 months: -20~25°C at 80%RH max; 3 months: -20~35°C at 80%RH max; 1 month: -43~45°C at 80%RH max | 58% SOC state |
| Average Weight | 664g±3.5% (semi-finished); 805g±3.5% (finished) | |
| Shell | Aluminum Plastic Film | |
| Appearance | No deformation, crack, burr, scratch, stain; surface dry and clearly marked | |
| Grouping Standard - Capacity Grade | 800mAh | |
| Grouping Standard - Voltage Grade | 10mV | |
| Grouping Standard - Internal Resistance Grade | 0.5mΩ | |
| Grouping Standard - K Value | ≤0.06mV/h |
| Item | Value | Tolerance | Note |
|---|---|---|---|
| Thickness (T) | 12.4 max mm (0% SOC, semi-finished); 13.0 max mm (58% SOC, finished) | ||
| Width (W) - Double Fold | 97.5 max mm | Battery width with double fold edge | |
| Width (W) - No Fold | 121.5 max mm | Battery width with no fold edge | |
| Length (L) | 318.5 max mm | Battery length | |
| Sealant Length (A) | 0.5~3.0 mm | Tab sealant exposed length | |
| Tab Width (B) | 70.0 mm | ±0.1 mm | |
| Tab Thickness | Aluminum 0.40 mm; Copper-nickel plated 0.30 mm | ±0.02 mm | |
| Top Sealing Width (C) | 14.0 mm | ±1.0 mm | |
| Tab Distance to Battery Edge (L1) | 13.5 mm | ±2.0 mm | |
| Tab Length (L2) | 22.0 mm | ±2.0 mm |
| Item | Condition | Result |
|---|---|---|
| Appearance | Visual inspection | No defects and no leakage |
| Dimension | Caliper for dimension | According to item 4 |
| Weight | Balance | According to item 3.3 |
| Shipment Voltage | Voltmeter, 58% SOC | 3.60~3.90V |
| Initial Internal Impedance | AC impedance at 1kHz, 58% SOC | ≤1.0mΩ |
| Discharge Capacity | Standard charge followed by standard discharge at 25±2°C | Minimum 55.0Ah |
| Cycle Life | 25±2°C, with splint, rest 30 min between cycles; charge 1.0C CC to 4.2V then 4.2V CV to 0.05C cut-off; discharge 1.0C CC to 2.75V | ≥80% of initial capacity after 800 cycles |
| Leakage Test | Fully charged, stored at 60±2°C and 85±5% RH for 7 days | No leakage |
| High/Low Temperature Discharge Characteristic | Charge 0.5C CC/CV to 4.2V, 0.05C cut-off at 25±2°C; discharge 0.5C CC to 2.2V at -20±2°C; discharge 0.5C CC to 2.75V at 55±2°C | ≥70% initial capacity at -20±2°C; ≥95% initial capacity at 55±2°C |
| External Short Circuit Test | Fully charged, short-circuited with 20mΩ resistor for 10 min at room temperature, observe 1 hour | No explosion and no fire |
| Over-Discharge Test | Fully discharged, 1C CC discharge for 90 min after standard charge, observe 1 hour | No explosion, no fire and no leakage |
| Overcharge Test | Fully charged, 1C CC charge to 1.1 times max charge voltage or 115% SOC, observe 1 hour | No explosion and no fire |
| Crush Test | Fully charged, half cylinder radius 75mm at ≤2mm/s, stop at 0V or 15% deformation or 100kN, observe 1 hour | No explosion and no fire |
| Drop Test | Fully charged, dropped from 1.0m onto concrete floor, observe 1 hour | No explosion, no fire and no leakage |
| Immersion Test | Fully charged, immersed in 3.5% NaCl solution for 2 hours | No explosion and no fire |
| Low Pressure Test | Fully charged, 11.6kPa, room temperature, 6 hours, observe 1 hour | No explosion, no fire and no leakage |
| Thermal Cycling Test | Fully charged, -40°C to 85°C cycling 5 times, observe 1 hour | No explosion, no fire and no leakage |
| Storage Performance | Stored 30 days at 25±2°C and 65±20% RH | Residual capacity ≥90% of initial capacity |
This battery is a rechargeable lithium-ion polymer product and must be used with a battery management system (BMS) that monitors, controls and protects each cell. The BMS shall include at least: charge termination at 4.20V, first-level overcharge protection at 4.22V, second-level overcharge protection at 4.25V with BMS lock-up, discharge cut-off, first-level over-discharge protection at 2.5V for 0°C < T ≤ 60°C and 2.2V for -20°C ≤ T ≤ 0°C, second-level over-discharge protection at 2.3V for 0°C < T ≤ 60°C and 2.0V for -20°C ≤ T ≤ 0°C with BMS lock-up, short circuit protection, over-current protection, over-temperature protection and charging time out protection within 8 hours.
\nStore the battery in a cool, dry and shady environment away from high temperature sources. For storage longer than one month, adjust SOC to around 60%. After three months of 60% SOC storage, charge and discharge once and adjust SOC back to around 60%. Do not store or transport the battery together with metal objects. The product shall be packed to prevent damage, and any conductive components contacting the two sealing edges must be insulated.
\nNever throw the battery into water or fire, never reverse the positive and negative terminals, never connect the positive and negative terminals with metal, never knock, throw or trample the battery, never directly solder the battery or pierce it with nails or other sharp tools, and never mix different types or models of lithium polymer batteries.
\n\nBrand: OID Manufacturer: Shenzhen Jianheng Technology Co Ltd (Jianheng) Certification: UN38.3, MSDS Place of Origin: China Minimum Order Quantity: 1 piece Supply Ability: 100,000 pieces per month Price: Contact us for preferential pricing Packaging: Standard export packaging with insulation protection Port: Shenzhen, China